Bond strength to micro-shearing in feldspathic ceramics conditioned with hydrofluoric acid and subjected to different removal times and methods
Descripción del Articulo
Objective: To evaluate the micro-shearing bond strength in feldspathic ceramics through various methods of hydrofluoric acid residue removal and different application times. Materials and methods: An in vitro study in which 9% hydrofluoric acid was applied for 1 minute as a surface treatment on feld...
| Autores: | , , , |
|---|---|
| Formato: | artículo |
| Fecha de Publicación: | 2025 |
| Institución: | Universidad Peruana Cayetano Heredia |
| Repositorio: | Revistas - Universidad Peruana Cayetano Heredia |
| Lenguaje: | español inglés |
| OAI Identifier: | oai:revistas.upch.edu.pe:article/6324 |
| Enlace del recurso: | https://revistas.upch.edu.pe/index.php/REH/article/view/6324 |
| Nivel de acceso: | acceso abierto |
| Materia: | ácido fluorhídrico cerámica resistencia al corte remoción de contaminantes agua destilada hydrofluoric acid ceramics shear strength contaminant removal distilled water ácido fluorídrico cerâmica resistência ao cisalhamento remoção de contaminantes água destilada |
| Sumario: | Objective: To evaluate the micro-shearing bond strength in feldspathic ceramics through various methods of hydrofluoric acid residue removal and different application times. Materials and methods: An in vitro study in which 9% hydrofluoric acid was applied for 1 minute as a surface treatment on feldspathic ceramic discs. The samples were divided into 4 groups with 3 different application times and subjected to different removal methods: water and air spray; ultrasonic bath with distilled water; active application of 37% phosphoric acid for 1, 2, and 4 minutes; and a combination of 37% phosphoric acid actively applied for 1, 2, and 4 minutes followed by an ultrasonic bath with distilled water for 4 minutes. Cylinders of flowable resin were prepared and placed on the ceramic discs. Samples were subjected to micro-shear tests on a semi-universal testing machine. Results: The two-way ANOVA test and Tukey's post-hoc test (p < 0.05) revealed that the water spray group at 1 and 2 minutes, and the ultrasonic bath at 4 minutes showed the highest bond strength values with a statistically significant difference. Conclusions: The water spray removal method for 1 and 2 minutes showed the highest bond strength value, while the lowest was observed with the 37% phosphoric acid removal method for 2 minutes. |
|---|
Nota importante:
La información contenida en este registro es de entera responsabilidad de la institución que gestiona el repositorio institucional donde esta contenido este documento o set de datos. El CONCYTEC no se hace responsable por los contenidos (publicaciones y/o datos) accesibles a través del Repositorio Nacional Digital de Ciencia, Tecnología e Innovación de Acceso Abierto (ALICIA).
La información contenida en este registro es de entera responsabilidad de la institución que gestiona el repositorio institucional donde esta contenido este documento o set de datos. El CONCYTEC no se hace responsable por los contenidos (publicaciones y/o datos) accesibles a través del Repositorio Nacional Digital de Ciencia, Tecnología e Innovación de Acceso Abierto (ALICIA).