Objective: Compare the surface roughness of two composite resins after immersion in carbonated beverages. Materials and methods: 160 resin discs (6 x 2 mm) were divided into 8 groups (n=20 per group) according to type of resin (Filtek™ Z350 XT® and Palfique LX5®) and type of immersion in beverages (...
Autores: | , |
---|---|
Formato: | artículo |
Fecha de Publicación: | 2024 |
Institución: | Universidad Científica del Sur |
Repositorio: | Revistas - Universidad Científica del Sur |
Lenguaje: | inglés |
OAI Identifier: | oai:revistas.cientifica.edu.pe:article/1834 |
Enlace del recurso: | https://revistas.cientifica.edu.pe/index.php/odontologica/article/view/1834 |
Nivel de acceso: | acceso abierto |
Materia: | surface roughness carbonated beverages Composite resins bebidas gaseosas resinas compuestas rugosidad superficial |
Sumario: | Objective: Compare the surface roughness of two composite resins after immersion in carbonated beverages. Materials and methods: 160 resin discs (6 x 2 mm) were divided into 8 groups (n=20 per group) according to type of resin (Filtek™ Z350 XT® and Palfique LX5®) and type of immersion in beverages (distilled water, Coca Cola®, Inca Kola® and Kola Escocesa®. The immersions were carried out under a structured cycle: 4 immersions a day for 5 days, intermediate storage in distilled water and overnight incubation for 8 h at 37°C. The measurements with the roughness meter were evaluated in three times: baseline, 7 and 14 days. The three-way Anova test was used at P<0.05. Results: Roughness showed differences only for the individual factors of time (P<0.000) and resin (P=0.000), and for the interaction time*drink (P=0.000) and resin*drink (P=0.003). Roughness was higher with Filtek Z350 XT® immersed with Inca Kola® (0.85 ± 0.37) than 14 days compared to other times (P=0.035) and with Palfique LX5 immersed in Coca Cola® at 7 days (1.61 ± 0.42) and in Inca Kola® at 14 days (1.66 ± 0.56) compared to distilled water (P<0,05). Conclusion: Surface roughness was affected by the type of resin, the type of soft drink and the immersion time. The roughness was greater with the Palfique LX5® nanohybrid resin, the Inca Kola® drink and after 14 days of immersion. |
---|
Nota importante:
La información contenida en este registro es de entera responsabilidad de la institución que gestiona el repositorio institucional donde esta contenido este documento o set de datos. El CONCYTEC no se hace responsable por los contenidos (publicaciones y/o datos) accesibles a través del Repositorio Nacional Digital de Ciencia, Tecnología e Innovación de Acceso Abierto (ALICIA).
La información contenida en este registro es de entera responsabilidad de la institución que gestiona el repositorio institucional donde esta contenido este documento o set de datos. El CONCYTEC no se hace responsable por los contenidos (publicaciones y/o datos) accesibles a través del Repositorio Nacional Digital de Ciencia, Tecnología e Innovación de Acceso Abierto (ALICIA).