Influence of Recycled Concrete and Ground Glass on the Compressive Strength of Concrete at 7 and 28 days
Descripción del Articulo
The main objective of the article is to assess the influence of using recycled aggregates on the compressive strength of concrete (f'c = 175 kg/cm2) at the age of 7 and 28 days. Specifically, the study focuses on the partial replacement of natural coarse and fine aggregates with recycled counte...
Autores: | , , |
---|---|
Formato: | artículo |
Fecha de Publicación: | 2025 |
Institución: | Universidad Peruana de Ciencias Aplicadas |
Repositorio: | UPC-Institucional |
Lenguaje: | inglés |
OAI Identifier: | oai:repositorioacademico.upc.edu.pe:10757/683814 |
Enlace del recurso: | http://hdl.handle.net/10757/683814 |
Nivel de acceso: | acceso embargado |
Materia: | ACI mix design Compressive strength Construction and demolition waste (CDW) Nonstructural elements Recycled aggregates Recycled concrete |
Sumario: | The main objective of the article is to assess the influence of using recycled aggregates on the compressive strength of concrete (f'c = 175 kg/cm2) at the age of 7 and 28 days. Specifically, the study focuses on the partial replacement of natural coarse and fine aggregates with recycled counterparts. To achieve this, recycled concrete from the demolition of columns in Villa el Salvador, Lima—Peru, was utilized as a substitute for the natural coarse aggregate. Additionally, ground glass sourced from glass shops in the Center of Lima was employed as a substitute for the natural fine aggregate. Three mixtures were designed following the ACI method: CC, representing conventional concrete; D1, denoting concrete with a 30% substitution (20% recycled concrete and 10% ground glass); and D2, indicating concrete with a 50% substitution (30% recycled concrete and 20% ground glass). Subsequent to the formulation of these mixtures, quality verification tests were conducted on the fresh concrete, and cylindrical specimens measuring 10 × 20 cm were created for sampling. After 7 days of curing, the specimens underwent compression tests, revealing strengths exceeding 65% of the design strength and after 28 days, strengths greater than 100% of the design strength. |
---|
Nota importante:
La información contenida en este registro es de entera responsabilidad de la institución que gestiona el repositorio institucional donde esta contenido este documento o set de datos. El CONCYTEC no se hace responsable por los contenidos (publicaciones y/o datos) accesibles a través del Repositorio Nacional Digital de Ciencia, Tecnología e Innovación de Acceso Abierto (ALICIA).
La información contenida en este registro es de entera responsabilidad de la institución que gestiona el repositorio institucional donde esta contenido este documento o set de datos. El CONCYTEC no se hace responsable por los contenidos (publicaciones y/o datos) accesibles a través del Repositorio Nacional Digital de Ciencia, Tecnología e Innovación de Acceso Abierto (ALICIA).