Influencia de la concentración de hidróxido de sodio y tiempo de lixiviación sobre el porcentaje de eliminación de arsénico presente en minerales auríferos refractarios usando lixiviación alcalina

Descripción del Articulo

ABSTRACT In the present research work, the influence is evaluated of the sodium hydroxide concentration and the time of operation on the percentage (%) of the removal of arsenic present in a refractory auriferous concentrate from the northern region of Peru, using leaching Alkaline. To carry out of...

Descripción completa

Detalles Bibliográficos
Autor: Zamalloa Barrera, Jorge Guillermo
Formato: tesis de maestría
Fecha de Publicación:2017
Institución:Universidad Nacional de Trujillo
Repositorio:UNITRU-Tesis
Lenguaje:español
OAI Identifier:oai:dspace.unitru.edu.pe:20.500.14414/12552
Enlace del recurso:https://hdl.handle.net/20.500.14414/12552
Nivel de acceso:acceso abierto
Materia:Minerales refractarios
Hidróxido de sodio
Lixiviación alcalina
Arsenopirita
Recuperación
id UNIT_f049c6d90dff181cdee8d509906d8660
oai_identifier_str oai:dspace.unitru.edu.pe:20.500.14414/12552
network_acronym_str UNIT
network_name_str UNITRU-Tesis
repository_id_str 4801
dc.title.es_PE.fl_str_mv Influencia de la concentración de hidróxido de sodio y tiempo de lixiviación sobre el porcentaje de eliminación de arsénico presente en minerales auríferos refractarios usando lixiviación alcalina
title Influencia de la concentración de hidróxido de sodio y tiempo de lixiviación sobre el porcentaje de eliminación de arsénico presente en minerales auríferos refractarios usando lixiviación alcalina
spellingShingle Influencia de la concentración de hidróxido de sodio y tiempo de lixiviación sobre el porcentaje de eliminación de arsénico presente en minerales auríferos refractarios usando lixiviación alcalina
Zamalloa Barrera, Jorge Guillermo
Minerales refractarios
Hidróxido de sodio
Lixiviación alcalina
Arsenopirita
Recuperación
title_short Influencia de la concentración de hidróxido de sodio y tiempo de lixiviación sobre el porcentaje de eliminación de arsénico presente en minerales auríferos refractarios usando lixiviación alcalina
title_full Influencia de la concentración de hidróxido de sodio y tiempo de lixiviación sobre el porcentaje de eliminación de arsénico presente en minerales auríferos refractarios usando lixiviación alcalina
title_fullStr Influencia de la concentración de hidróxido de sodio y tiempo de lixiviación sobre el porcentaje de eliminación de arsénico presente en minerales auríferos refractarios usando lixiviación alcalina
title_full_unstemmed Influencia de la concentración de hidróxido de sodio y tiempo de lixiviación sobre el porcentaje de eliminación de arsénico presente en minerales auríferos refractarios usando lixiviación alcalina
title_sort Influencia de la concentración de hidróxido de sodio y tiempo de lixiviación sobre el porcentaje de eliminación de arsénico presente en minerales auríferos refractarios usando lixiviación alcalina
author Zamalloa Barrera, Jorge Guillermo
author_facet Zamalloa Barrera, Jorge Guillermo
author_role author
dc.contributor.advisor.fl_str_mv Cárdenas Alayo, Ranulfo Donato
dc.contributor.author.fl_str_mv Zamalloa Barrera, Jorge Guillermo
dc.subject.es_PE.fl_str_mv Minerales refractarios
Hidróxido de sodio
Lixiviación alcalina
Arsenopirita
Recuperación
topic Minerales refractarios
Hidróxido de sodio
Lixiviación alcalina
Arsenopirita
Recuperación
description ABSTRACT In the present research work, the influence is evaluated of the sodium hydroxide concentration and the time of operation on the percentage (%) of the removal of arsenic present in a refractory auriferous concentrate from the northern region of Peru, using leaching Alkaline. To carry out of the test, the samples of concentrate of 200 g (20% solids) in a volume of 1 L. and with a grain size of -325 mesh (45um), at a temperature of 80°C, with addition of air and agitation, were subjected to different concentrations of sodium hydroxide 1.25 M, 1.5 M, and 1.75 M., and at different operating time levels of 1.5hrs. 2.5hrs. and 3.5hrs. to obtain the maximum percentage (%) of arsenic removal, using alkaline leaching. The mineralogical study of the sample of refractory gold concentrate concluded that despite having studied three polished sections to have a larger study area, no native gold grain or free gold minerals were observed, which reinforces the belief that gold occurs As a solid solution within arsenopyrite or pyrite or both (Annex B). The final results obtained show that at a concentration of 1.25M and with an operating time of 3.5 hrs., the maximum percentage (%) of arsenic removal of 59.78% was obtained, leaving the residue with a 2.18% arsenic law. From the above, and based on the statistical analysis carried out, it can be stated that the sodium hydroxide concentration and the operating time significantly influence the percentage (%) of arsenic removal from the refractory auriferous concentrate.
publishDate 2017
dc.date.accessioned.none.fl_str_mv 2019-05-21T15:18:28Z
dc.date.available.none.fl_str_mv 2019-05-21T15:18:28Z
dc.date.issued.fl_str_mv 2017
dc.type.es_PE.fl_str_mv info:eu-repo/semantics/masterThesis
format masterThesis
dc.identifier.uri.none.fl_str_mv https://hdl.handle.net/20.500.14414/12552
url https://hdl.handle.net/20.500.14414/12552
dc.language.iso.es_PE.fl_str_mv spa
language spa
dc.relation.ispartof.fl_str_mv SUNEDU
dc.rights.es_PE.fl_str_mv info:eu-repo/semantics/openAccess
dc.rights.uri.es_PE.fl_str_mv http://creativecommons.org/licenses/by-nc-nd/2.5/pe/
eu_rights_str_mv openAccess
rights_invalid_str_mv http://creativecommons.org/licenses/by-nc-nd/2.5/pe/
dc.publisher.es_PE.fl_str_mv Universidad Nacional de Trujillo
dc.source.es_PE.fl_str_mv Universidad Nacional de Trujillo
Repositorio institucional - UNITRU
dc.source.none.fl_str_mv reponame:UNITRU-Tesis
instname:Universidad Nacional de Trujillo
instacron:UNITRU
instname_str Universidad Nacional de Trujillo
instacron_str UNITRU
institution UNITRU
reponame_str UNITRU-Tesis
collection UNITRU-Tesis
bitstream.url.fl_str_mv https://dspace.unitru.edu.pe/bitstreams/d952f091-65ed-47e0-ba40-988bcdbc6897/download
https://dspace.unitru.edu.pe/bitstreams/bd9d0741-b98c-4ac3-9be6-d77f5d8dc857/download
bitstream.checksum.fl_str_mv 3ea6eab2d59d173f71f7665175c98083
8a4605be74aa9ea9d79846c1fba20a33
bitstream.checksumAlgorithm.fl_str_mv MD5
MD5
repository.name.fl_str_mv Repositorio Institucional - UNITRU
repository.mail.fl_str_mv repositorios@unitru.edu.pe
_version_ 1807290128093151232
spelling Cárdenas Alayo, Ranulfo DonatoZamalloa Barrera, Jorge Guillermo2019-05-21T15:18:28Z2019-05-21T15:18:28Z2017https://hdl.handle.net/20.500.14414/12552ABSTRACT In the present research work, the influence is evaluated of the sodium hydroxide concentration and the time of operation on the percentage (%) of the removal of arsenic present in a refractory auriferous concentrate from the northern region of Peru, using leaching Alkaline. To carry out of the test, the samples of concentrate of 200 g (20% solids) in a volume of 1 L. and with a grain size of -325 mesh (45um), at a temperature of 80°C, with addition of air and agitation, were subjected to different concentrations of sodium hydroxide 1.25 M, 1.5 M, and 1.75 M., and at different operating time levels of 1.5hrs. 2.5hrs. and 3.5hrs. to obtain the maximum percentage (%) of arsenic removal, using alkaline leaching. The mineralogical study of the sample of refractory gold concentrate concluded that despite having studied three polished sections to have a larger study area, no native gold grain or free gold minerals were observed, which reinforces the belief that gold occurs As a solid solution within arsenopyrite or pyrite or both (Annex B). The final results obtained show that at a concentration of 1.25M and with an operating time of 3.5 hrs., the maximum percentage (%) of arsenic removal of 59.78% was obtained, leaving the residue with a 2.18% arsenic law. From the above, and based on the statistical analysis carried out, it can be stated that the sodium hydroxide concentration and the operating time significantly influence the percentage (%) of arsenic removal from the refractory auriferous concentrate.RESUMEN En el presente trabajo de investigación, se evalúo la influencia de la concentración de hidróxido de sodio y el tiempo de operación sobre el porcentaje (%) de eliminación de arsénico presente en un concentrado aurífero refractario proveniente de la región norte del Perú, empleando la lixiviación alcalina. Para la realización de las pruebas, las muestras de concentrado de 200 g (20% de sólidos) en un volumen de 1 L., con una granulometría de malla -325 (45um), a una temperatura de 80°C, con adición de aire y agitación, se sometieron a diferentes concentraciones de hidróxido de sodio 1.25 M, 1.5 M., y 1.75 M y a diferentes niveles de tiempo de operación de 1.5hrs. 2.5hrs., y 3.5hrs., para obtener el máximo porcentaje (%) de eliminación de arsénico, usando la lixiviación alcalina. El estudio mineralógico de la muestra de concentrado aurífero refractario concluyó, que a pesar de haber estudiado tres secciones pulidas para tener mayor superficie de estudio no se ha observado ningún grano de oro nativo o minerales de oro libre lo cual refuerza la creencia que el oro ocurre como solución sólida dentro de la arsenopirita o pirita o en ambos (Anexo B). Los resultados finales obtenidos muestran que, a una concentración de 1.25M y con un tiempo de operación de 3.5 hrs., se obtuvo el máximo porcentaje (%) de eliminación de arsénico de 59.78%, quedando el residuo con una ley de 2.18% de arsénico. De lo propuesto anteriormente y en base al análisis estadístico efectuado se puede afirmar que la concentración de hidróxido de sodio y el tiempo de operación influyen notablemente en el porcentaje (%) de eliminación de arsénico del concentrado aurífero refractario.TesisspaUniversidad Nacional de Trujilloinfo:eu-repo/semantics/openAccesshttp://creativecommons.org/licenses/by-nc-nd/2.5/pe/Universidad Nacional de TrujilloRepositorio institucional - UNITRUreponame:UNITRU-Tesisinstname:Universidad Nacional de Trujilloinstacron:UNITRUMinerales refractariosHidróxido de sodioLixiviación alcalinaArsenopiritaRecuperaciónInfluencia de la concentración de hidróxido de sodio y tiempo de lixiviación sobre el porcentaje de eliminación de arsénico presente en minerales auríferos refractarios usando lixiviación alcalinainfo:eu-repo/semantics/masterThesisSUNEDUMaestríaMaestro en CienciasMaestría en Ciencias mención Gestión AmbientalUniversidad Nacional de Trujillo.Escuela de PosgradoORIGINALZamalloa Barrera Jorge Guillermo.pdfZamalloa Barrera Jorge Guillermo.pdfapplication/pdf2491558https://dspace.unitru.edu.pe/bitstreams/d952f091-65ed-47e0-ba40-988bcdbc6897/download3ea6eab2d59d173f71f7665175c98083MD51LICENSElicense.txtlicense.txttext/plain; charset=utf-81748https://dspace.unitru.edu.pe/bitstreams/bd9d0741-b98c-4ac3-9be6-d77f5d8dc857/download8a4605be74aa9ea9d79846c1fba20a33MD5220.500.14414/12552oai:dspace.unitru.edu.pe:20.500.14414/125522019-05-21 10:18:28.769http://creativecommons.org/licenses/by-nc-nd/2.5/pe/info:eu-repo/semantics/openAccessopen.accesshttps://dspace.unitru.edu.peRepositorio Institucional - UNITRUrepositorios@unitru.edu.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
score 13.936249
Nota importante:
La información contenida en este registro es de entera responsabilidad de la institución que gestiona el repositorio institucional donde esta contenido este documento o set de datos. El CONCYTEC no se hace responsable por los contenidos (publicaciones y/o datos) accesibles a través del Repositorio Nacional Digital de Ciencia, Tecnología e Innovación de Acceso Abierto (ALICIA).